CERESResearch Repository

High-temperature challenges: electrochemical investigations into molten salt corrosion mechanisms

dc.contributor.authorYu, Fuzhen
dc.contributor.authorNicholls, John R.
dc.contributor.authorAria, Adrianus Indrat
dc.contributor.authorSyed, Adnan U.
dc.date.accessioned2026-04-21T10:12:00Z
dc.date.available2026-04-21T10:12:00Z
dc.date.freetoread2026-04-21
dc.date.issued2026-03
dc.date.pubOnline2026-03-15
dc.descriptionThis article belongs to the Special Issue Alloy Materials Degradation and Microstructural Study
dc.description.abstractThermal energy storage (TES) systems are widely employed in concentrated solar power (CSP) applications as a means of storing and dispatching energy. Typical thermal fluids used in TES systems include molten salts, such as solar salt (a KNO3–NaNO3 eutectic), as well as other inorganic salts currently under consideration. While these molten nitrate, chloride, sulfate, and carbonate salts offer favourable thermal properties, they can induce significant corrosion of metallic containment materials, leading to reduced system efficiency and component lifetime. Despite extensive post-exposure studies, in situ electrochemical understanding of corrosion mechanisms in molten solar salt remains limited, particularly for emerging alloys such as FeCrAl. In this study, the in situ corrosion behaviour of structural alloys in molten solar salt was investigated using electrochemical impedance spectroscopy (EIS). Complementary post-exposure characterization was performed using destructive techniques, including scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDX), to assess microstructural and chemical changes. The materials evaluated were stainless steel SS316 and comparatively underexplored Kanthal FeCrAl alloys, exposed to molten solar salt (40 wt% KNO3–60 wt% NaNO3) at 545 °C. The electrochemical and microstructural analyses indicate that FeCrAl exhibits superior corrosion resistance associated with the formation of a more stable and protective oxide scale, compared to SS316 under the investigated conditions. This study provides new electrochemical evidence supporting the suitability of FeCrAl alloys for TES applications, while also indicating that SS316 may develop improved corrosion resistance over extended exposure durations, highlighting the importance of long-term performance assessment.
dc.description.journalNameCrystals
dc.identifier.citationYu F, Nicholls JR, Aria AI, Syed AU. (2026) High-temperature challenges: electrochemical investigations into molten salt corrosion mechanisms. Crystals, Volume 16, Issue 3, March 2026, Article number 200en_UK
dc.identifier.eissn2073-4352
dc.identifier.elementsID870156
dc.identifier.issn2073-4352
dc.identifier.issueNo3
dc.identifier.paperNo200
dc.identifier.urihttps://doi.org/10.3390/cryst16030200
dc.identifier.urihttps://dspace.lib.cranfield.ac.uk/handle/1826/25117
dc.identifier.volumeNo16
dc.languageEnglish
dc.language.isoen
dc.publisherMDPIen_UK
dc.publisher.urihttps://www.mdpi.com/2073-4352/16/3/200
dc.rightsAttribution 4.0 Internationalen
dc.rights.urihttp://creativecommons.org/licenses/by/4.0/
dc.subjectconcentrating solar power (CSP)en_UK
dc.subjectthermal energy storage (TES)en_UK
dc.subjectmolten salt corrosionen_UK
dc.subjectelectrochemical characterizationen_UK
dc.subjectsolar salten_UK
dc.subject34 Chemical Sciencesen_UK
dc.subject7 Affordable and Clean Energyen_UK
dc.subject3402 Inorganic chemistryen_UK
dc.titleHigh-temperature challenges: electrochemical investigations into molten salt corrosion mechanismsen_UK
dc.typeArticle
dc.type.subtypeArticle
dcterms.dateAccepted2026-03-10

Files

Original bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
Salt_Corrosion_Mechanisms-2026.pdf
Size:
1.57 MB
Format:
Adobe Portable Document Format
Description:
Published version

License bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
license.txt
Size:
1.63 KB
Format:
Plain Text
Description: